About Cobalt Based Investment Casting Process
The ceramic mildew is preheated to all-around one thousand°C (1832°File) prior to molten metal is poured to the mould cavity. The metal is allowed to cool and solidify into the final condition.The wax pattern is then melted, leaving a cavity inside the stucco material in The form of the pattern. Molten metal is poured into this cavity. After the